Classification:

EN ISO 18274

AWS A5.14

S Ni 6082 (NiCr20Mn3Nb)

ERNiCr-3

Description:

Cromamig 82 is intended for welding Inconel 600, Incoloy 800 and similar composition nickel base

alloys particularly where these are used for high temperature service. Highly suitable for a wide range

of dissimilar joint combinations between nickel base alloys, Monels, mild and low alloy steels and

austenitic stainless steels. Can be used to clad carbon steels with an Inconel type surface. Suitable

for welding 5% and 9% nickel steels for cryogenic applications.

Welding current:

DC+

Mechanical properties

Shielding gas:

I1, Ar 99.99%, 16-21 l/min

I3, Ar + 30% He, 20-25 l/min

Yield strength, Rp0.2%:

Tensile Strength, Rm:

Elongation, A5

Impact energy, CV:

Typical

Wire composition, wt.%





























400 MPa

660 MPa

35%

20°C • 150 J

–196°C • 80 J

Corrosion resistance

Very good resistance to general and intergranular

corrosion. Very good resistance to stress

corrosion cracking.

² Nb + Ta

Scaling temperature:

The weld metal is resistant to oxidation

– in air up to 1150°C

– in sulphur dioxide up to 800°C

– in hydrogen sulphide up to 550°C

Product data:

Diam. Product code

mm

1,0

1,2

98182010

98182012

Spool weight



15 kg S300

15 kg S300

75-140

130-160

164

  

18-21

18-21

170-200

175-250

26-28

26-28