Page 55
53
Classification:
EN ISO 3580-A
E CrMo2 B 42 H5
AWS A5.5 E 9018-B3
Description:
P 84CR is a basic-coated, low hydrogen electrode which deposits a low carbon 2.25% Cr/1.0% Mo
weld metal. It is intended for welding creep resisting steels of similar composition, used in steam
generation plant operating at temperatures up to 600°C, e.g. EN 10CrMo9-10, EN 11CrMo9-10,
ASTM 335 Gr. P22, ASTM 217 Gr WC9. Also suitable for use in the chemical and petrochemical
industries where resistance to hydrogen attack, corrosion from sulphur bearing crude oil and stress
corrosion cracking in sour environments is required. Preheat and interpass temperature of 200-250°C
is recommended. Post-weld heat treat at 690°C.
Coating type:
Basic
Metal recovery:
110-120%
Welding positions:
Welding current:
DC+
Redrying temperature:
350-400°C, 2h
Chemical composition, wt.%
Mechanical properties
Typical
Yield strength, Rp0.2%: N/A**
Tensile Strength, Rm: N/A**
Elongation, A5 N/A**
Impact energy, CV: N/A**
Hydrogen content / 100 g weld metal
≤ 5 ml
Product data
2,5 350 71842500
65-100 22 0,72 71 0,8
3,2 350 71843200
90-150 23 0,73 37 1,4
4,0 350 71845000
130-200 24 0,73 19 1,8
5,0 450 71845000
160-265 25 0,73 12 2,6