Classification:

E Ni 6182

EN ISO 14172

AWS A5.11

E NiCrFe-3

Description:

Cromarod 82 is a basic flux coated nickel-base electrode intended for welding Inconel 600 and similar

composition alloys. The deposit tolerates high dilution levels and is very resistant to hot cracking. It is

not susceptible to sigma phase embrittlement or carbon migration and is therefore ideal for service at

elevated temperatures.

Cromarod 82 is highly suitable for a wide range of dissimilar joint combinations between nickel-base

alloys, Monels, mild and low alloy steels and austenitic stainless steels. It can also be used to clad

carbon steels with an Inconel type surface. The weld metal exhibits very good fracture toughness at

temperatures down to -196 °C and is suitable for welding 5% and 9% nickel steels for cryogenic

applications.

Coating type:

Basic

Mechanical properties

Welding positions:

Yield strength, Rp0.2%:

Tensile Strength, Rm:

Elongation, A5

Impact energy, CV:

Typical



Welding current:

DC+

Redrying temperature:

350 °C, 2h

380 MPa

630 MPa

39%

-196 °C • 80 J

Ferrite content:

FN 0 (WRC-92)

Chemical composition, wt.%

























Corrosion resistance

Very good resistance to general and intergranular

corrosion. Very good resistance to stress

corrosion cracking.

High temperature properties:

The weld metal is resistant to oxidation

– in air up to 1100 °C

Approvals:

CE

Product data

  









2,5

300

74542500

45-70

25-27

3,2

350

74543200

70-110

25-27





85







